A liquid sulfur dioxide battery, such as K/KCl SbCl₅ (0.25
molar) + IBr₃ (15 %wt) + SO₂ (1)/carbon matrix is shown to have an
open circuit voltage greater than 3.70 volts and an initial voltage of
3.15 volts, decreasing to 2.40 volts in 10 minutes at a current density
of...
The pore size distribution of several battery separators were
determined experimentally by mercury penetration method using the
Aminco-Winslow porosimeter. The performances of the separators under
electrolyte penetration were also studied. The results of electrolyte
penetration revealed that the degree of penetration was affected
by the anions of the entrained salts...