Ti-6Al-2Sn-4Zr-2Mo-0.1Si specimens were shaped by repeated cycles of heating
(to 954 °C) and hammer or press forging followed by a solution anneal that varied from
968 to 998 °C. The coupons were originally extracted from billets forged below the beta
trans us ( 1009 °C) and slow cooled to ambient...