Joints were fabricated from different combinations of untreated and fire-retardant- treated (FRT) Douglas-fir dimension lumber and 3/8-inch plywood. Eight types of fasteners and three fire-retardant treatments were tested. Joint specimens were exposed 2 and 7 years in cold, standard, and warm-humid conditions, then tested in lateral bearing. Best overall performance...
Fifteen large glued-laminated beams made from visually graded hem-fir lumber were designed, fabricated, and tested to failure in static bending. When tested, the beams had an average moisture content of 7.5 percent. The beams were 40 feet long, 5 1/8 inches wide and 24 inches deep. Before laminating, individual pieces...